AerMet® 100 provides high hardness and ultra-high strength combined with exceptional ductility and fracture toughness. The alloy has a minimum tensile strength of 1930 MPa (280 ksi) and a minimum fracture toughness of 100 ksi.
AerMet® 100 provides high hardness and ultra-high strength combined with exceptional ductility and fracture toughness. The alloy has a minimum tensile strength of 1930 MPa (280 ksi) and a minimum fracture toughness of 100 ksi.
The exceptional combination of hardness, toughness, tensile strength and ductility makes this alloy a candidate for aerospace applications including landing gear, engine shafts and drive shafts.
AerMet® 100 may be considered for use up to about 427°C.
PRODUCT FORM | SIZE RANGE FROM | SIZE RANGE TO |
---|---|---|
AerMet® 100 round bar | 15.88 mm | 203.2 mm |
Density: 7.89 g/cm³
Melting Range: °C
Hardness: 51-55.5 HRC
Specific Heat Capacity: J/kg.°C
Electrical Resistivity: 0.43 µΩ.m
Curie Temperature: °C
Fastners
Landing Gear
Actuators
Ordnance
Ballistic Tolerant Components
Jet Engine Shafts
Drive Shafts
Our AERMET 100 is carefully handled to minimize damage during storage and transportation and to preserve the quality of the product in its original condition.