Nitronic 32 alloy is a nitrogen strengthened, low nickel austenitic stainless steel that is characterized by excellent fabricability and corrosion resistance, and high strength at both ambient and elevated temperatures. In addition, the alloy offers good ductility even at high strengths.
Nitronic 32 alloy is a nitrogen strengthened, low nickel austenitic stainless steel that is characterized by excellent fabricability and corrosion resistance, and high strength at both ambient and elevated temperatures. In addition, the alloy offers good ductility even at high strengths. Hence, the alloy serves as an ideal material for manufacturing cold-headed parts that require high mechanical properties.
Coil - Contact Ulbrich Sales
Wire - Profile, Round, Flat, Square
Element | Content (%) |
---|---|
Chromium, Cr | 16.5 - 19.5 |
Manganese, Mn | 11-14 |
Silicon, Si | 1 |
Nickel, Ni | 0.5-2.5 |
Nitrogen, N | 0.2-0.45 |
Carbon, C | 0.15 |
Phosphorus, P | 0.06 |
Sulfur, S | 0.03 |
Iron, Fe | Balance |
Properties | Metric | Imperial |
---|---|---|
Density | 7.83 g/cm3 | 0.283 lb/in3 |
Melting point | 1450-1510°C | 2642-2750°F |
Properties | Metric | Imperial |
---|---|---|
Tensile strength | 690 MPa | 100000 psi |
Yield strength | 379 MPa | 55000 psi |
Elongation at break | 30% | 30% |
Rockwell B hardness | 92 | 92 |
Properties | Metric | Imperial |
---|---|---|
Thermal expansion co-efficient (@23-93°C/73-200°F) | 16.16 µm/m°C | 8.98 µin/in°F |